DefectCommon causeRemedy
PorosityMoisture, dirt, poor gasDry, clean, check gas
CrackHydrogen, fast coolingDry basic electrode, follow preheat procedure
UndercutHigh current, fast travelReduce and pause at edges
Lack of fusionLow current, wrong angleIncrease, aim at the joint
Slag inclusionPoor cleaningBrush between passes